2023-01-11 16:56:34
2022-09-06 10:34:35
2022-09-06 10:30:49
2023-02-15 10:13:32
Our inspector arrived at the factory and started regular project testing.
1. Material
Use of recycled material can result in excessive swelling, delamination and warping,
our inspector will observe the flooring material color, smell etc. to judge whether factory using virgin/ recycle material.
2. Appearance and Size, Number
- Defects, fissures, wrinkles, holes, Offset printing, delamination, peeling, Gloss unevenness, Press mark, Spots, bubbles, scratches, discoloration etc.
- Length, Width, Thickness
- Patent sticker
- Order number and Loading Number
After check over, all items looks good. Then factory without any test equipment because it's new.
3. Physical and Chemical Performance Requirements
The SPC flooring process machines are automatic, which greatly improve the production efficiency, but the stability of the control of the floor is difficult
to increase, so we will do the spc testing as follow:
1. Dimensional changes after heating( 6hrs at 80℃)
2. Curl after 6hrs at 80℃
3. Fitting degree (film paper and SPC core)
4. Density test
5. Tensile strength test
6. Ply Adhesion
7. Abrasion resistance
8. Surface scratch resistance
9. Hardness test
10. Customized test
We take back the samples and spent a lot of time to test the flooring performance to ensure the flooring quality.
We will try our best to ensure our customer benefit, assist them to find issues, solve issues.